供应PA66美国杜邦105 阻燃级,耐候标准产品
价格:45起
产品规格:
产品数量:
包装说明:
关 键 词:PA66美国杜邦105
行 业:塑料 通用/工程塑料 工程塑料
发布时间:2022-08-22
供应PA66美国杜邦105 阻燃级,耐候标准产品
产品参数
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 |
| 基本性能 | 吸水率 | 饱和(23℃) | ASTM D-570 |
|
|
| DAM|50%RH |
|
|
|
|
| 8.5|- |
|
|
|
|
|
| % |
|
|
|
| 吸水率 | 24小时浸渍(23℃) | ASTM D-570 |
|
| DAM|50%RH |
|
|
|
| 1.2|- |
|
|
|
| % |
|
|
|
|
| 物理性能 | 比重 |
| ASTM D-792 |
|
| DAM|50%RH |
|
|
|
|
| 1.15|1.15 |
|
|
|
|
|
|
|
|
|
| 机械性能 | 屈服强度 | 23℃ |
|
|
| DAM|50%RH |
|
|
|
| 90.3|62.1 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
| MPa |
|
|
|
| 屈服伸长率 |
| ASTM D-638 |
|
| DAM|50%RH |
|
|
|
| 5|25 |
|
|
|
| % |
|
|
|
| 断裂伸长率 | 23℃ | ASTM D-638 |
|
| DAM|50%RH |
|
|
|
| 30|200 |
|
|
|
| % |
|
|
|
| 埃佐冲击强度 | 23℃ | ASTM D-256 |
|
| DAM|50%RH |
|
|
|
| 43|107 |
|
|
|
| j/m |
|
|
|
| 拉伸强度 | 23℃ | ASTM D-638 |
|
| DAM|50%RH |
|
|
|
| 90.3|62.1 |
|
|
|
| MPa |
|
|
|
| 洛氏硬度R |
| ASTM D-785 |
|
| DAM|50%RH |
|
|
|
| R121|R109 |
|
|
|
|
|
|
|
| 洛氏硬度M |
| ASTM D-785 |
|
| DAM|50%RH |
|
|
|
| M87|M80 |
|
|
|
|
|
|
|
| 剪切强度 | 23℃ | ASTM D-732 |
|
| DAM|50%RH |
|
|
|
| 72.4|68.9 |
|
|
|
| MPa |
|
|
|
| 揉曲模量 | 23℃ | ASTM D-790 |
|
| DAM|50%RH |
|
|
|
| 2964|1310 |
|
|
|
| MPa |
|
|
|
|
| 电气性能 | 耗散因数 | 103Hz(cps) | ASTM D-150 |
|
| DAM|50%RH |
|
|
|
| 0.03|0.12 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
| 介电常数 | 103Hz(cps) | ASTM D-150 |
|
| DAM|50%RH |
|
|
|
| 3.9|7.0 |
|
|
|
|
|
|
|
| 耗散因数 | 106Hz(cps) | ASTM D-150 |
|
| DAM|50%RH |
|
|
|
| 0.03|0.08 |
|
|
|
|
|
|
|
| 耗散因数 | 100Hz(cps) | ASTM D-150 |
|
| DAM|50%RH |
|
|
|
| 0.02 |0.13 |
|
|
|
|
|
|
|
| 介电常数 | 106Hz(cps) | ASTM D-150 |
|
| DAM|50%RH |
|
|
|
| 3.6|4.6 |
|
|
|
|
|
|
|
| 介电常数 | 100Hz(cps) | ASTM D-150 |
|
| DAM|50%RH |
|
|
|
| 4.0|8.0 |
|
|
|
|
|
|
|
| 体积电阻率 |
| ASTM D-257 |
|
| DAM|50%RH |
|
|
|
| 1014|1012 |
|
|
|
| Ω.cm |
|
|
|
|
| 热性能 | 脆化温度 |
| ASTM D-746 |
|
| DAM|50%RH |
|
|
|
| -52|-52 |
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
| ℃ |
|
|
|
| 热畸变温度 | 18×106Pa | ASTM D-648 |
|
| DAM|50%RH |
|
|
|
| 90|- |
|
|
|
| ℃ |
|
|
|
| 荷重形变 | 13.8Mpa 50℃ | ASTM D-621 |
|
| DAM|50%RH |
|
|
|
| 1.2|- |
|
|
|
| % |
|
|
|
| 热畸变温度 | (0.5)×106Pa | ASTM D-648 |
|
| DAM|50%RH |
|
|
|
| 240|- |
|
|
|
| ℃ |
|
|
|
| UL可燃性导级 |
| UL 94 |
|
| DAM|50%RH |
|
|
|
| 94|V-2 |
|
|
|
|
|
|
|
| 熔点 | Fisher Johns法 | ASTM D-789 |
|
| DAM|50%RH |
|
|
|
| 255|255 |
|
|
|
| ℃ |
|
|
|
|
| 其它性能 | 需氧指数 |
| ASTM D-2863 |
|
| DAM|50%RH |
|
|
|
|
| 25|31 |
|
|
|
|